Why does the coal chute tee wear through so frequently? CCO Welded overlay plates extend pipeline service life
The coal chute tee is the most vulnerable part of the pulverized coal pipeline, where wear is most severe and failures occur most frequently.
Rapid wear is caused by three factors:
*Swirling flows and concentrated impact
*Hard quartz impurities grinding the wall
*Coal lumps striking with high kinetic energy.
Wear rate here can be 3-5 times higher than straight pipes, with over 60% of failures occurring at this point. Ordinary carbon steel or manganese steel tees often wear through within weeks or months, leading to leakage, pollution, and costly unplanned shutdowns.
HISAN wear resistant tees, made from HS200 10+10 high-chromium carbide overlay wear plates (hardness ≥HRC58, Cr ≥32%), provide strong bonding, impact resistance, and superior anti-abrasion performance. They resist swirling erosion, particle grinding, and coal lump impact simultaneously, greatly extending service life and reducing maintenance frequency. Under normal conditions, service life can reach 3-5 years; in harsher environments, customized selection is recommended to maximize performance.)